Method for judging the results of salt spray test


The purpose of salt spray test is to evaluate the quality of salt spray corrosion resistance of goods or metal materials. The results of salt spray test are the judgment of product quality and the key to correctly measuring the quality of salt spray corrosion resistance of goods or metals. The methods for judging the results of salt spray tests include rating method, weighing method, corrosion judgment method, and corrosion data statistical analysis method.
 
1、 The connection between salt spray test and practice
 
Artificial simulation of salt spray environment test is a testing equipment with a certain capacity space - salt spray test chamber. Artificial methods are used in its capacity space to evaluate the salt spray corrosion resistance and quality of products in salt spray environment. Compared with the natural environment, the salt content of fluoride in salt spray environment can be several times or tens of times higher than that in general natural environment, greatly increasing the corrosion rate. The salt spray test on the product significantly reduces the time required for the results. If testing product samples in a naturally exposed environment, corrosion may take up to 1 year, while testing under artificial simulated salt spray conditions can obtain similar results in just 24 hours.
 
The artificial simulated salt spray test also includes neutral salt spray test, acetic acid salt spray test, copper salt accelerated acetic acid salt spray test, and alternating salt spray test.
 
1. Neutral salt spray test (NSS test) is currently the most widely used accelerated corrosion test method in the field of application. Select 5% sodium chloride solution and adjust the pH value of the solution in the neutral range (6-7) as the spray solution. The experimental temperature is 35 ℃, and the salt spray settling rate is between 1-2ml/80cm2. h.
 
2. Acetate salt spray test (ASS test) should be developed under the premise of neutral salt spray test. This is to add some acetic acid to a 5% sodium chloride solution, making it possible for the solution to become acidic when the pH value drops to 3, and the resulting salt spray changes from neutral salt spray to acidic. Its corrosion rate is about three times faster than the NSS test.
 
3. Copper salt accelerated acetate salt spray test (CASS test) is a rapid salt spray corrosion test developed recently abroad. The test temperature is 50 ℃, and a small amount of copper salt copper chloride is added to the solution to strongly induce corrosion. Its corrosion rate is about 8 times that of the NSS test.
 
4. Alternating salt spray test is a comprehensive salt spray test, which is actually a neutral salt spray test and a stability cold and humidity test. Mainly used for internal cavity products of the whole machine. Salt spray corrosion occurs not only on the surface of the product, but also inside the product through infiltration in a humid environment. This is to replace and convert products under salt spray and cold and humid environmental conditions, and ultimately evaluate whether the mechanical strength and performance of the entire product have changed.
 
2、 Factors affecting salt spray corrosion
 
The main factors affecting the salt spray test results include: test temperature and humidity, salt solution concentration, sample placement angle, solution pH, salt spray sedimentation, spray method, etc.
 
1. Test temperature and humidity
 
Temperature and relative humidity affect the corrosion effect of salt spray. The critical relative humidity for metal corrosion is about 70%. When the relative humidity reaches or exceeds the critical humidity, salt is prone to deliquescence, producing electrolytes with good conductivity. When the relative humidity decreases, the concentration of the solution will increase until the crystalline salt precipitates, and the corrosion rate will correspondingly decrease.
 
The higher the salt spray corrosion rate, the faster the test temperature. International Organization for Standardization IEC60355:1971《ANAPPRAISALOFTHEPROBLEMSOFACCELERATEDTESTINGFORATMOSPHERICCORROSION》 The standard states that for every 10 ℃ increase in temperature, the corrosion rate increases by 2-3 times and the electrolyte conductivity increases by 10-20%. This is because as the temperature rises, molecular motion intensifies and the rate of chemical change accelerates. For the neutral salt spray test, most scholars believe that a test temperature of 35 ℃ is more suitable. If the test temperature is too high, the mechanism of salt spray corrosion will vary greatly from the specific situation.
 
2. Salt solution concentration
 
The effect of salt solution concentration on corrosion rate is related to the type of material and coating. When the concentration is below 5%, the corrosion rate of steel, nickel, and brass increases with the increase of concentration; When the concentration is greater than 5%, the corrosion rate of these metals decreases with increasing concentration. This situation can be explained by the oxygen content in the solution. The oxygen content in the solution is related to the concentration of salt. In the low concentration range, the oxygen content increases with the increase of salt content. However, when the salt concentration increases to 5%, the oxygen content reaches relative saturation. If the salt content continues to increase, the oxygen content will correspondingly decrease. When the oxygen content decreases, the depolarization ability of oxygen decreases, that is, the corrosion effect weakens. But for metals such as zinc, cadmium, and copper, the corrosion rate always increases with the increase of solution concentration.
 
3. Perspective of sample placement
 
The placement angle of the sample has a significant impact on the results of the salt spray test. The settling direction of salt spray is close to the vertical direction. When the sample is placed horizontally, its expansion area is the largest, and the salt spray on the surface of the sample is the highest, so the corrosion is the most severe. The research results show that when the steel plate forms 45 angles with the horizontal line, the corrosion loss weight per square meter is 250g, and when the steel plate plane is parallel to the vertical line, the corrosion weight is 140g per square meter. The GB/T2423.17-93 standard stipulates that "the placement method of flat samples should make the test surface form a 30 degree angle with the vertical direction
 
4. pH value of the solution
 
One of the main factors affecting the results of salt spray tests is the pH of the solution. The lower the concentration of hydrogen ions in a pH solution, the stronger the acidity and corrosiveness. The salt spray test of Fe/Zn, Fe/Cd, Fe/Cu/Ni/Cr and other electroplated parts shows that the corrosiveness of the acetic acid salt spray test (ASS) is 1.5 to 2.0 times more severe than that of the pH value of 6.5 to 7.2. The neutral salt spray test (NSS) is 1.5 to 2.0 times more severe.
 
The pH of the solution may change due to environmental factors. Therefore, both domestic and international salt spray test standards have an impact on the pH range of the solution, and under stable test conditions, the pH of the solution is proposed to improve the reproducibility of the salt spray test results.
 
5. Salt fog sedimentation and spray mode
 
The finer the salt spray particles, the larger the surface area formed, the greater the amount of adsorbed oxygen, and the stronger the corrosiveness. More than 90% of salt spray particles in nature have a diameter of 1 μ m. The scientific research results are as follows: the oxygen content adsorbed on the surface of salt spray particles with a diameter of 1 μ m is relatively balanced with the oxygen content dissolved inside the particles. No matter how small the salt spray particles are, the adsorbed oxygen content will not increase.
 
Traditional spraying methods include air pressure spraying and tower spraying. The main drawbacks of salt spray settling are poor uniformity and large particle diameter. The ultrasonic atomization method utilizes the principle of ultrasonic atomization to directly atomize the solution into salt spray, and diffuses it into the experimental area, solving the problem of poor uniformity of salt spray settlement and smaller particle diameter of salt spray. Different spraying methods can also affect the pH value
 
3、 Salt spray test standards and judgment of test results
 
Standards are unified regulations for repetitive things and brief descriptions. The salt spray test standard refers to the conditions of the salt spray test, such as temperature, humidity, concentration of sodium chloride solution, and pH. In addition, technical standards are proposed for the performance of the salt spray test chamber. Select the salt spray test standard for the same product based on the characteristics of the salt spray test, metal corrosion rate, and sensitivity to salt spray.
 
The following are the standards for salt spray testing, such as GB/T2423.17-1993 Basic Environmental Testing Procedures for Electronic and Electrical Products Test Ka: Salt Spray Test Method, GB/T2423.18-2000 Environmental Testing for Electronic and Electrical Products Part 2 Kb: Salt Spray, Alternating (Sodium Chloride Solution), GB5938-86 "Corrosion Resistance Test Method for Metal Coatings and Chemical Treatment Layers of Light Industrial Products" GB/T1771-91 "Determination of Neutral Salt Spray Resistance of Paints and Varnishes".
 
The purpose of salt spray test is to evaluate the quality of salt spray corrosion resistance of goods or metal materials. The results of salt spray test are the judgment of product quality and the key to correctly measuring the quality of salt spray corrosion resistance of goods or metals.
 
The methods for judging the results of salt spray tests include rating method, weighing method, appearance method of corrosive substances, and statistical analysis method of corrosion data.
 
The rating judgment method is to divide the percentage of corrosion area to total area into several levels according to a certain method, and use a certain level as the basis for qualified judgment, which is suitable for evaluating flat samples;
 
2. The weighing judgment method is to determine the corrosion resistance quality of a sample by weighing the weight of the sample before and after the corrosion test, and calculating the weight of the corrosion loss. It is particularly suitable for evaluating the corrosion resistance quality of a certain metal;
 
3. The determination method of corrosive substances is a qualitative method. It judges the sample based on whether the product undergoes corrosion after the salt spray corrosion test. This method is mainly used for general product standards;
 
4. The statistical analysis method of corrosion data has brought methods for designing corrosion tests, analyzing corrosion data, and determining the confidence range of corrosion data. It is mainly used for analyzing and statistical analysis of corrosion status, rather than the quality of specific products
 
Mainly suitable for artificial simulated salt spray environment testing in industries such as hardware, electroplating, electronic components, chemical coatings, baking paint, automotive, screws, springs, organic and inorganic films, anodizing, rust prevention oil, etc.
 
If multiple climate tests are completed using the same specimen, in the vast majority of cases, it is recommended to conduct salt spray tests after other tests. Salt deposits can interfere with the results of other experiments. Generally, the same specimen is not used for salt spray, mold, and wet heat tests. If necessary, salt spray tests should also be conducted after mold and wet heat tests.
 
4、 Salt spray test judgment criteria
 
1. GB/T 6461-2002 Rating of test specimens and test pieces for metal and other inorganic coatings on metal substrates after corrosion testing;
 
2. ISO 10289-1999 Rating of test specimens and parts for corrosion testing of metal and other inorganic coatings on metal parts;
 
It is divided into 11 levels (0~10).
 
Level 10: Defect free area, appearance rating A, no change in sample surface appearance;
 
Level 9: The defect area does not exceed 0.1%, the appearance rating is B, and there is slight to moderate discoloration on the surface of the sample;
 
Level 8: The proportion of defect area ranges from 0.1% to 0.25%, with an appearance rating of C. The surface of the sample is severely discolored or has very slight corrosion;
 
Grade 7: Defect area accounts for 0.25%~0.5%, appearance rating is D, severe loss of gloss or extremely mild corrosion products on the surface of the sample;
 
Level 6: Defect area accounts for 0.5%~1.0%, appearance rating is E, severe loss of gloss on the surface of the sample, or thin layers of corrosion products or pitting on the local surface of the sample;
 
Level 5: Defect area accounts for 1.0%~2.5%, appearance rating F, there are corrosion products or pitting corrosion on the surface of the sample, and one of them is distributed throughout the surface of the sample;
 
Level 4: Defect area accounts for 2.5% to 5%, appearance rating G, and there is a thick layer of corrosion products or pitting corrosion on the surface of the sample;
 
Level 3: Defect area accounts for 5% to 10%, appearance rating is H, there is a very thick layer of corrosion products or pitting corrosion on the surface of the sample, and there are deep pitting corrosion;
 
Level 2: Defect area accounts for 10%~25%, appearance rating I, and the sample shows corrosion of the base metal;
 
Level 1: Defect area accounts for 25% to 50%, indicating severe corrosion.
 
Level 0: If the defect area accounts for more than 50%, it belongs to a very serious corrosion phenomenon.
 
3. ASTM D1654-2008 Standard Test Method for Evaluation of Painted or Coated Specimens in Corrosive Environments.